Did I mess up bedliner application?

Arrowhead

Oldtimer
I undercoated the entire underside of the fiberglass Cobra and everything went great and hardened up no problem. BUT, there were four small aluminum panels I also shot the next day and they are still soft. I think the problem was the panels were too cold (didn't pre heat the garage enough). It's been over two weeks and they are still soft. I thought heat might help so I put them in the boiler room where it's probably 80 degees but they are still kind of soft after about 5 days. Is that helping or should I just scrape it off and recoat? It really isn't a big deal if I have to redo them, they are flat and not very big.

(YES, I USED THE GEO GUN AND MIXED CORRECTLY)
 
Arrowhead;34505 said:
I undercoated the entire underside of the fiberglass Cobra and everything went great and hardened up no problem. BUT, there were four small aluminum panels I also shot the next day and they are still soft. I think the problem was the panels were too cold (didn't pre heat the garage enough). It's been over two weeks and they are still soft. I thought heat might help so I put them in the boiler room where it's probably 80 degees but they are still kind of soft after about 5 days. Is that helping or should I just scrape it off and recoat? It really isn't a big deal if I have to redo them, they are flat and not very big.

(YES, I USED THE GEO GUN AND MIXED CORRECTLY)

Did they finally harden up or did you strip them?

Steve
 
Back
Top