I'm only asking because I want to prevent this from happening to my SPI Epoxy when I apply it.
The area photographed shows bubbles in the paint itself, which turn into rust spots under the primer. the spots go away when sanded. I don't think any go through the metal. I don't know what type of primer this is... just that there is ALOT of it! I bought this hood used from someone who doesn't know its history.
These spots, and larger areas of flash rust, exist under the filler everywhere on the panel, even when the little blisters aren't visible.
Any thoughts?
The area photographed shows bubbles in the paint itself, which turn into rust spots under the primer. the spots go away when sanded. I don't think any go through the metal. I don't know what type of primer this is... just that there is ALOT of it! I bought this hood used from someone who doesn't know its history.