I'm new to this forum and new to spi products. I've had good luck with intercoat clear. Struggled a bit today with my first run with UV clear. Started out with medium activator, but switched right away to slow and just couldn't get it to flow good. Had a hard time keeping a wet edge. Seemed like I couldn't get across the hood with getting dry overspray when I went back to the fender where I started. Results were overall good, but had to really smash it on. Turned out on material an additional 1/2 turn (3 turns out total) but OS got excessive so I dropped pressure from 29 to 25 at the gun... W400 bellaria 1.4. Seemed good out of the gun, but really dried fast. Almost no tack in 20 min. Booth temp was about 80. Humidity was low and was running dryer in the shop. I am in the habit of warming clear... Material was about 90 degrees. The only other thing is the air compressor is in another room and it was pretty hot in there. Good news is I couldn't make it run if I tried!!! Is this clear just really temp sensitive? Any advise before I wet sand and reclear would be appreciated. I'm not really of the mind set of thinning clear either... Don't care for adding more solvents.