I should have been more clear. Mix the rage ultra extra with rage ultra 50/50, then add normal amount of hardenerLOL, I do agree Rage Ultra is superior to the Gold but I think mixing 50/50 is going to be a shocking experience.
John
I apologize. I missed the "Extra" in the Rage Ultra Extra which gives the added work time. I guess I sounded like a smart a$$. That was not my intention.
John
I wish I could trade summer weather with you, but not the winter The low last night was 83, and the humidity was horrible. Sprayed a Dodge 3500 crew cab Friday (less the roof) with Euro mixed 4:1:1 with slow hardener, 895, and 2 caps retarder in 28oz. By the time I got around it, where I started was barely tacky. Started second coat immediately, and by the time I got around it, the clear didn't want to melt in to to the back of the cab where I started. Amazing what this heat and humidity does to all these materials.Since we don't deal with extreme heat for much of the year, the strategy here is to simply come in early and do any filler work first thing, before it gets ugly.