I noticed when doing a spot clear repair (now redoing whole panel) that the unsanded new uv clear had much more gloss that what was cut and buffed. I hard blocked runs with 600 then 800 followed by 1000 all over up through grits to 3000. I used a rotary buffer with wool pad and cg v32 which really brought out the color and shine. Next was da orange pad with cg v36 , cg v38. Looking at it in the sun looks great with no scratches. I usually make 3-4 passes at each step and with the buffer I am nervous about overdoing it. Should I work more on any step or?