Experimentation working with retarder. 4:1:1, slow hardener, 895. 3-4 capfuls per quart when added at 90°+. Over 100° I start replacing the 895 with retarder, keeping the reducer at the same ratio (4:1:1). Up to 115°+ half reducer, half retarder. That hot sprays similar to 4:1:1 with 895 and a few caps of retarder at 90°. Sprayed a mirror first coat at 4:1:1 half and half 895/retarder. Second coat 4:1:.5 straight retarder. Slick! Still a little tacky after 30 minutes.