Had an issue with solvent pop on my last three pieces,not horrible but it's there. First time this has occurred on my project.
Only difference was higher temperature, 80 degrees and all other work was done at 70ish and not a problem.
Waited 35 minutes between base coats, three total -Nason Ful base 3.5 activated(Only solvent base we can buy here). Sealed with SPI epoxy, hour flash before base and then three coats of Universal with normal activator, 30 minutes between coats.
Any idea what I did wrong---too high a temperature, not enough flash time?
Whats the best way to fix this? Sand it all off and start over I'm assuming?
Not beaten, just a little discouraged
Thanks as always.
Dean
Only difference was higher temperature, 80 degrees and all other work was done at 70ish and not a problem.
Waited 35 minutes between base coats, three total -Nason Ful base 3.5 activated(Only solvent base we can buy here). Sealed with SPI epoxy, hour flash before base and then three coats of Universal with normal activator, 30 minutes between coats.
Any idea what I did wrong---too high a temperature, not enough flash time?
Whats the best way to fix this? Sand it all off and start over I'm assuming?
Not beaten, just a little discouraged
Thanks as always.
Dean